Product Name: | HDPE Geomembrane Liner |
Thickness: | 0.2mm-3.0mm(Main:0.5mm, 0.75mm,1.0mm,1.5mm,2.0mm) |
Length : | 50m/roll,100m/roll,150m/roll or follow your request |
width: | 1m-8m or follow customers' demand, Main width is 4m,5m,5.8m,6.0m |
Surface | Both side smooth/both side textured one side textured one side smooth, or as your request |
Color: | White,Black,Green,Blue,mainly black |
Material: | 97.5% HDPE and 2.5% Carbon black content |
Certification: | ISO9001:2008,CE |
Standard: | GB-T 17643-2011 , CJ/T _234-2006 , ASTM GRI-GM13 |
S/N | Item | Index | ||||||
Thickness mm | 0.75 | 1.00 | 1.25 | 1.50 | 2.00 | 2.50 | 3.00 | |
1 | Density g/cm3 | |||||||
2 | Tensile yield strength (Vertical and Horizontal ) N/mm |
≥11 | ≥15 | ≥18 | ≥22 | ≥29 | ≥37 | ≥44 |
3 | Tensile breaking strength (vertical and horizontal ) N/mm |
≥20 | ≥27 | ≥33 | ≥40 | ≥53 | ≥67 | ≥80 |
4 | Elongation (vertical and horizontal ) % | - | - | - | ≥12 | |||
5 | Elongation at break (vertical and horizontal ) % |
≥700 | ||||||
6 | Tearing load at right angle ( Vertical and horizontal ) N |
≥93 | ≥125 | ≥160 | ≥190 | ≥250 | ≥315 | ≥375 |
7 | Anti-puncture strength N | ≥240 | ≥320 | ≥400 | ≥480 | ≥540 | ≥800 | ≥960 |
8 | Tensile load stress cracking (Tensile method of deal load of the cut ) h | - | ≥300 | |||||
9 | Carbon black content % | 2.0-3.0 | ||||||
10 | Carbon black dispersion | The number of level 3 among 10 data is not more than one: Level 4 and Level 5 are not allowed | ||||||
11 | Oxidation induction time ( OIT) min | Oxidation induction time under normal pressure ≥100 | ||||||
Oxidation induction time under disjoining pressure ≥400 | ||||||||
12 | 85ºC thermal aging (retention rate of OIT under normal pressure after 90d ) % | ≥55 | ||||||
13 | Ultraviolet resistance (retention rate of OIT after 1600 h ultraviolet irradiation ) % | ≥50 | ||||||
Note : Technical performance index of thickness specification not listed in the table shall be implemented according to interpolation method . | ||||||||
For two indexes of Item 11 and Item 13 , select one from retention rate of OIT under normal pressure and retention rate of OIT under high pressure and carry out the test |
Qingdao Qianmiao International Trading Co.,Ltd ,which are professional in producing various Geomembrane waterproof materias in China for over 5 years .Currently mainly products we have HDPE /LDPE/EVA/PVC waterproof materias Geomembrane .
We have three Geomembrane producing line machine in our factory .The capacity of prodce is up to 10000000 ton per year
So that we can guarantee the deliever goods on time.
The All the geomembrane materias are strictly prodcued by GB/T17643-2011,CJ/T234-2006 ,GRI-GM13 Stardar.
Therefore,the quality of Geomembrane can meet your require , you can be rest assured
At the same time we can produce the Geomembrane as the clients' demand.
Due to good quality and best service ,we get the well reputation from all the world clients.
Welcome to vist us and build the cooperation with each other for long time
Contact information
Contact person : Tony